Huawei Gas beetle cutting trolley is a oxygen flame gas cutter. It is supplied with a main aluminum body, 1pcs flat rail, 1pcs cutting torch assembly, 1 set of circling-cutting parts and 3pcs propane or acetylene cutting tips. This beetle cutting trolley is widely used because of its simplicity, low price and easy operation.
The differences between CG1-30 and CG1-100
The main differences between CG1-30 and CG1-100 is the quantity of cutting torch assembly. CG1-30 has a single cutting torch, however, CG1-100 has double cutting torch. Both machines are semi-automatic oxy-fuel cutting machines, and multi-use machines with Acetylene as its flame gas.
The differences between CG1-30A and CG1-30B
The main differences between CG1-30A and CG1-30B is the working rail. 30A is with “H” rail, 30B is with hole rail. The rail is different, the driving wheels and directional wheels will be different, the price also will be different. So please show us the exact needs, then can supply you the correct pug cutting trolley.
Item Model | CG1-30A、CG1-30B | CG1-100A、 CG1-100B |
Steel plate thickness | 8-100mm | 8-100mm |
Cutting speed | 50-750mm/min | 50-750mm/min |
Cutting circle Diameter | φ200-2000mm | φ200-2000mm |
Cutting thickness | 6-100mm | 6-100mm |
Power | Ac220v,50Hz | Ac220v,50Hz |
Machine body dimension | 470*230*240 | 470*230*240 |
Weight | Small vehicle 15 kg,guide rail,radius 12kg |
Small vehicle 18 kg,Track Radius bar 12 kg |
Functions of cutting trolley
The surface cutting roughness could reach to 12.5 and needless to cutting processing further on common occasion. The mainly function of this flame cutting machine is to do straight linear cutting. It has an additional function to do circling-cutting as well as V shape beveling. What’s more, If more facilities added, it can even be used for quench and plastic welding. For an example, adding a oscillator with CG1-30, then can do welding job.
Details of Huawei Gas Cutting Trolley
The cutting torch assembly with 2 different hoses to distinguish the connected hoses, red color and blue color. There is a quick valve to control the cutting functions, not need to open or close the small valves to adjust the gas for working. The control plate has two different designs, one is big, the other one is small. Our Huawei gas cutting trolley is with big control plate. However, if you want to get more competitive machine, small control plate and without quick valve are available.
How to select the wanted cutting tips?
Different sizes of the cutting tips, different cutting thickness. First confirm the needed cutting thickness, then select the corresponding cutting nozzles. See below detailed parameter of G02 (acetylene)and G03 (propane)tips.
Type | No. | Gas cutting aperture(mm) |
Cutting Thickness(mm) |
Cutting speed (mm/min) |
Oxygen pressure(Mpa) |
Acetylene pressure(Mpa) |
Acetylene GO₂ |
#00 | 0.8 | 5-10 | 600-450 | 0.2-0.3 | >0.03 |
#0 | 1.0 | 10-20 | 480-380 | 0.2-0.3 | 0.03 | |
#1 | 1.2 | 20-30 | 400-320 | 0.25-0.35 | 0.03 | |
#2 | 1.4 | 30-50 | 350-280 | 0.25-0.35 | 0.03 | |
#3 | 1.6 | 50-70 | 300-240 | 0.3-0.4 | 0.04 | |
#4 | 1.8 | 70-90 | 260-200 | 0.3-0.4 | 0.04 | |
#5 | 2 | 90-120 | 210-170 | 0.4-0.6 | 0.04 | |
#6 | 2.4 | 120-160 | 180-140 | 0.5-0.8 | 0.05 | |
#7 | 2.8 | 160-200 | 150-110 | 0.6-0.9 | 0.05 | |
#8 | 3.2 | 200-280 | 90-60 | 0.6-1.0 | 0.05 | |
#9 | 3.6 | 270-350 | 90-60 | 0.7-1.1 | 0.05 | |
#10 | 4 | 350-400 | 70-50 | 0.7-1.2 | 0.06 |
Type | No. | Gas cutting aperture(mm) |
Cutting thickness(mm) |
Cutting speed (mm/min) |
Oxygen pressure(Mpa) |
Acetylene pressure(Mpa) |
Propane GO3 |
#0 | 0.7 | 5-10 | 800-450 | 0.2-0.3 | >0.03 |
#1 | 0.9 | 10-20 | 480-300 | 0.2-0.3 | 0.03 | |
#2 | 1.2 | 20-35 | 400-320 | 0.3-0.4 | 0.03 | |
#3 | 1.5 | 35-60 | 350-280 | 0.3-0.4 | 0.03 | |
#4 | 1.8 | 60-90 | 300-240 | 0.4-0.6 | 0.04 | |
#5 | 2.1 | 90-130 | 260-200 | 0.4-0.6 | 0.04 | |
#6 | 2.5 | 130-180 | 220-180 | 0.4-0.6 | 0.04 | |
#7 | 2.7 | 180-250 | 200-160 | 0.5-0.7 | 0.05 | |
#8 | 3.1 | 250-330 | 180-140 | 0.5-0.7 | 0.05 | |
#9 | 3.5 | 330-380 | 130-90 | 0.6-0.8 | 2.05 | |
#10 | 4.0 | 380-450 | 90-50 | 0.6-0.8 | 0.05 |
Can these Huawei Gas Cutting Trolley do circling-cutting and plasma cutting?
Yes, they can. Our standard machines are with the circling-parts to do extra circling cutting, including their main straight-line cutting function. What’s more, the plasma cutting also is available.
Common problems and trouble shooting Guide
No. | Symptom | Possible caused | Possible solution |
1 | No power supply of vehicle after power Connecting |
1:No electricity from the power socket 2:Fuse is burn up 3:shedding wire in socket plug and switch |
1:Examine and repair the circuit 2:Replace the fuse 3:Fix the shedding wire |
2 | Motor is not working after power connection but voltage is normal |
1:Connection problem between the socket and plug of the motor 2:Move less of the motor bus 3:Motor magnet falls to stop armature working |
1:Weld the shedding wire and correctly connect the socket,repair the connecting slice when necessary 2:Take out of the brush and mill it to ensure good connection 3:Replace the motor |
3 | Speed of the vehicle can not be adjusted |
Slide connection problem of the potentiometer | Repair the slide or replace the potentiometer |
4 | Gas leakage between the cutting torch and cutting tip |
1:Nut is not fastened firmly enough 2:Copper rust and dirt on conical surface of the cutting torch 3:Dirt or damage on the conical surface of the cutting tip |
1:Fasten the nut firmly 2:Clean the copper rust and dirty by sand paper 3:Clean the dirt by sand paper,replace the tip it necessary |
5 | Flame goes out once oxygen valve is open |
Cutting oxygen leaking to oxygen preheating area 1:Copper rust and dust on conical surface of inner side of the cutting torch 2:Dirt or damage on the conical surface of the cutting tip |
1:Clean the copper rust and dirt by sand paper 2:Clean the dirt by sand paper,replace the cutting tip if necessary |
6 | Steel plate can not be cut totally enough |
1:Small size of the cutting tip 2:Less power of flame 3:Less pressure of the cutting oxygen 4:Jam of the cutting oxygen pipe 5:Low purity of the oxygen 6:Oxygen leaking to oxygen-preheating area |
1:Choose suitable size of the cutting tip based on cutting thickness 2:Properly increase the power of the flame 3:Properly increase the pressure of the cutting oxygen to ensure enough flowing speed and force 4:Clean the dust inside the oxygen pipe 5:Use oxygen with purity more than 95% 6:Clean the dirt on cutting torch and cutting tip and mil the damaged conical surface,Replace the cutting tip when necessary |
7 | Cutting edge is not straight | 1:Steel place is not placed on the same level or the steel plate is distorted 2:Shifting blowing direction of the flame 3:The track is not placed on the same level |
1:Place the steel plate flatly and adjust before cutting 2:The cutting torch should be vertical to the steel plate and fastened firmly.Clean the dust inside the tip 3:Adjust the track of the vehicle |